MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Ineos N12Z-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: N12Z-00 impact copolymer polypropylene is a medium melt flow rate, nucleated and antistatic product designed for injection molding applications. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.
    Applications:
  • Housewares, consumer goods including storage container and lids
  • Appliance housings
  • Rigid packing requiring exceptional toughness
  • Material handling products (crates and pails)
    Benefits:
  • High impact resistance
  • Very good stiffness
  • Excellent mold release
  • Good static dissipation

Information provided by Ineos Olefins & Polymers USA

Key Words: Medium melt flow rate, nucleated and antistatic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.903 g/cc0.0326 lb/in³ASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 6666ASTM D785
Tensile Strength at Break 18.0 MPa2610 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 22.5 MPa3260 psi2.0 in/min; ASTM D638
Elongation at Break 380 %380 %2.0 in/min; ASTM D638
Elongation at Yield 6.6 %6.6 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1060 MPa154000 psiASTM D790A
Izod Impact, Notched 0.908 J/cm
@Temperature -20.0 °C
1.70 ft-lb/in
@Temperature -4.00 °F
ASTM D256
Izod Impact, Notched (ISO)  8.90 kJ/m²
@Temperature -20.0 °C
4.24 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.9 °C201 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C127 °FUnannealed; ASTM D648
Vicat Softening Point 144 °C291 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 68 %68 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Dynatup Instrumented ImpactDuctile23°C, mode of failure
 Ductile-20°C, mode of failure
ProcessInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem 5E16S Polypropylene Homopolymer
Ineos 3950 Polypropylene Impact Copolymer
Braskem 52T30V Homopolymer Polypropylene
BP Amoco Amoco® Polypropylene Homopolymer
Borealis RF926MO Polypropylene, Transparent Random Copolymer

PINEOS909 / 130368

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.