MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical GY-FROP40 Halogen-Free Synthetic Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP) is a leading manufacturer of specialty chemicals in Asia. We devote ourselves to supplying products and solutions to our customers worldwide to satisfy and expand the market needs. GY-FR-OP40 is a highly-effective halogen-free synthetic flame retardant that can provide long-term flame retardant effect for end products. It can be applied to various plastics, polymers, resins, elastomers, foam materials, adhesives, etc. In addition to the characteristics of low specific gravity and low corrosivity, GY-FR-OP40 also provides excellent thermal decomposition temperature to minimize the volume of the smoke. It is also a prevailing flame retardant designated for use by major factories in the world.

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. (GYC GROUP) is a leading manufacturer of specialty chemicals in Asia. We devote ourselves to supplying products and solutions to our customers worldwide to satisfy and expand the market needs. GY-FR-OP40 is a highly-effective halogen-free synthetic flame retardant that can provide long-term flame retardant effect for end products. It can be applied to various plastics, polymers, resins, elastomers, foam materials, adhesives, etc. In addition to the characteristics of low specific gravity and low corrosivity, GY-FR-OP40 also provides excellent thermal decomposition temperature to minimize the volume of the smoke. It is also a prevailing flame retardantdesignated for use by major factories in the world.

Advantages:

  • Provides excellent long term flame retard effect
  • Non-halogen (no Fluorine, Chlorine, Bromine, halogen element) flame retardant
  • Reduces the volume of the smoke
  • Provides excellent thermal decomposition temperature
  • Low specific gravity and corrosion/ low density smoke
  • Compatible with all kinds of plastic, polymer, resin, elastomer, foam, adhesive compounding
Applications:
  • Thermal setting resin: epoxy resin, phenol resin, unsaturated resin, polyester resin, acrylic resin, etc.
  • Coating and various resin: Flame retard coating, powder coating, acrylic products, polyurethane resin, PMMA, latex resin, adhesive related products
  • Thermoplastic plastic: PP, PS, PE, EVA, PA, PET, PC, POLYOLIFIN, POLYESTER RESIN, NYLON, POM, PBT, engineering plastic, etc.
  • Rubber and elastomer industries: All kinds of natural and synthetic rubber: TPE, SBS, SEBS
  • PU synthetic leather, TPU artificial leather
  • Various of foam and flame retard foaming products
  • Polyamide like (polyamide 66, 6, 11, 12)
  • Polyurethanes type (TPU, PU resin) of electronic products made from TPU: switches, connectors, and covers
  • Non-solvent coatings

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
pH 5.5 - 6.55.5 - 6.5
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 350 °C662 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
 
Descriptive Properties
AppearanceRefined Powder
ColorWhite
TypeHalogen-free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN002 / 266310

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.