MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Syensqo (Solvay Specialty Polymers) Amodel® AT-6115 HS PPA, 15% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: 15% glass fiber, impact modified, high flow, hot-water molds, heat stabilized

Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. This grade was developed for automotive snap-fit electronic connectors. It offers high flow and short molding cycles.

- Black: AT-6115 HS BK 324
- Natural: AT-6115 HS NT

Markets/Uses: Automotive / Automotive E/E / Actuators Bus Bars; Electric Vehicles; Engine Sensors; EV Recharger Connectors; Sensors; Solenoids; Wire Harness Connectors; Fuel Flanges; Rollover Valves

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Connectors; Housings; Industrial Applications; Industrial Parts; Machine/Mechanical Parts; Metal Replacement; Valves/Valve Parts

Features: Fast Molding Cycle; Good Mold Release; Heat Stabilized; High Elongation; High Flow; Impact Modified; Lubricated

Injection notes: Injection Rate: 2 to 4 in/sec
Holding Pressure: 50% of injection pressure
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³Method A; ISO 1183
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 126 MPa18300 psiISO 527-2
Tensile Strength 122 MPa17700 psiASTM D638
Elongation at Break 3.4 %3.4 %ASTM D638
 4.1 %4.1 %ISO 527-2
Tensile Modulus 5.20 GPa754 ksiISO 527-2
 5.38 GPa780 ksiASTM D638
Flexural Strength 165 MPa23900 psiASTM D790
 66.9 MPa
@Temperature 100 °C
9700 psi
@Temperature 212 °F
ISO 178
 170 MPa
@Temperature 23.0 °C
24700 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 4.41 GPa640 ksiASTM D790
 2.34 GPa
@Temperature 100 °C
339 ksi
@Temperature 212 °F
ISO 178
 4.27 GPa
@Temperature 23.0 °C
619 ksi
@Temperature 73.4 °F
ISO 178
Compressive Strength 100 MPa14500 psiASTM D695
Shear Strength 56.5 MPa8190 psiASTM D732
Izod Impact, Notched 0.910 J/cm1.70 ft-lb/inASTM D256
Izod Impact, Unnotched 8.50 J/cm15.9 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²Type 1, Notch A; ISO 180
Izod Impact, Unnotched (ISO) 55.0 kJ/m²26.2 ft-lb/in²Type 1; ISO 180
Charpy Impact Unnotched 7.60 J/cm²36.2 ft-lb/in²Type 1, Edgewise; ISO 179
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  22.0 µm/m-°C
@Temperature 0.000 - 100 °C
12.2 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
 30.0 µm/m-°C
@Temperature 100 - 200 °C
16.7 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
CTE, linear, Transverse to Flow  90.0 µm/m-°C
@Temperature 0.000 - 100 °C
50.0 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
 120 µm/m-°C
@Temperature 100 - 200 °C
66.7 µin/in-°F
@Temperature 212 - 392 °F
ASTM E831
Melting Point 305 °C581 °FPeak; ASTM D3418
 305 °C581 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 298 °C568 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 251 °C484 °FUnannealed; ISO 75-2/A
 260 °C500 °FAnnealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 316 - 324 °C601 - 615 °F
Front Barrel Temperature 327 - 332 °C621 - 630 °F
Melt Temperature 321 - 335 °C610 - 635 °FInjection
Mold Temperature 66.0 - 93.0 °C151 - 199 °F
Drying Temperature 110 °C
@Time 14400 sec
230 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer; Impact Modifier; Lubricant; Mold Release
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingWater-Heated Mold Injection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4105 / 279905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.