MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® F161 Epoxy Resin, 120 Kevlar Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Hexcel designation: 120-38"-F161; Fiber: Kev. 49 195

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Filler Content 44.0 %Laminate Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 190 MPa
@Temperature 177 °C
Wet
 238 MPa
@Temperature 177 °C
Dry
 259 MPa
@Temperature 132 °C
Wet
 334 MPa
@Temperature 132 °C
Dry
 393 MPa
@Temperature -54.0 °C
Dry
 399 MPa
@Temperature 24.0 °C
Wet
 410 MPa
@Temperature 24.0 °C
Dry
Tensile Modulus 17.9 GPa
@Temperature 177 °C
Wet
 18.6 GPa
@Temperature 132 °C
Wet
 19.0 GPa
@Temperature 177 °C
Dry
 21.9 GPa
@Temperature 132 °C
Dry
 24.9 GPa
@Temperature 24.0 °C
Wet
 25.9 GPa
@Temperature 24.0 °C
Dry
 27.3 GPa
@Temperature -54.0 °C
Dry
Compressive Yield Strength 52.0 MPa
@Temperature 177 °C
Wet
 70.0 MPa
@Temperature 132 °C
Wet
 90.0 MPa
@Temperature 177 °C
Dry
 117 MPa
@Temperature 132 °C
Dry
 139 MPa
@Temperature 24.0 °C
Wet
 199 MPa
@Temperature 24.0 °C
Dry
 222 MPa
@Temperature -54.0 °C
Dry
Compressive Modulus 14.0 GPa
@Temperature 177 °C
Wet
 15.7 GPa
@Temperature 132 °C
Wet
 16.9 GPa
@Temperature 177 °C
Dry
 18.4 GPa
@Temperature 132 °C
Dry
 21.0 GPa
@Temperature 24.0 °C
Wet
 24.1 GPa
@Temperature -54.0 °C
Dry
 26.8 GPa
@Temperature 24.0 °C
Dry
Shear Strength 15.0 MPa
@Temperature 132 °C
Short Beam
 16.0 MPa
@Temperature 177 °C
Short Beam
 19.0 MPa
@Temperature 177 °C
Short Beam
 26.0 MPa
@Temperature 132 °C
Short Beam
 34.0 MPa
@Temperature -54.0 °C
Short Beam
 34.0 MPa
@Temperature 24.0 °C
Short Beam
 36.0 MPa
@Temperature 24.0 °C
Short Beam
 
Descriptive Properties
Cured Thickness per Ply (cm)0.01Laminate
Dry Resin Content (%)52-58Prepreg
Flow (%)20-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Solvay CYCOM® 985 Epoxy + Kevlar 49 Fiber Laminate
Hexcel® HexPly® F185 Epoxy Resin, 120 Glass Fabric

PHEXC111 / 98581

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.