MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultramid® A3K R01 Nylon 66, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Product Description: Ultramid® A3K R01 is an unreinforced easy flowing, injection molding grade PA66. Applications; Typical applications include fast processing high stress technical parts or electrically insulating parts.

Availability: Asia Pacific; Europe; Europe; North America

Features: Electrically Insulating; Fast Molding Cycle; Good Flow

Use: Electrical Parts; Electronic Insulation

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Forms: Pellets

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccISO 1183
Maximum Moisture Content 0.20
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 7250 psiISO 527-2
Elongation at Break >= 50 %ISO 527-2
Elongation at Yield 20 %ISO 527-2
Tensile Modulus 160000 psiISO 527-1
Charpy Impact Unnotched NB
@Temperature -40.0 °C
ISO 179
 NB
@Temperature 22.8 °C
ISO 179
Charpy Impact, Notched 9.50 ft-lb/in²ISO 179
 
Processing PropertiesOriginal ValueComments
Mold Temperature 104 - 179 °F
Drying Temperature 176 °F
Dry Time 2.00 - 4.00 hour
Back Pressure 508 - 1810 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2074 / 310767

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.