MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Henkel Loctite® Stycast® 2762FT with CAT 17 Epoxy Encapsulant
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Loctite Stycast 2762FT provides the following product characteristics:
  • High temperature resistance
  • High thermal conductivity
  • Excellent chemical resistance
  • Low coefficient of thermal expansion
  • Low shrinkage

Cure: Room temperature or Heat cure

Application: Potting, Encapsulant

Loctite Stycast 2762FT epoxy encapsulant is designed for potting electronic components exposed to harsh environments. This material is also ideal for large and complex castings that require high temperature resistance and thermal conductivity.

Loctite Stycast 2762FT can be used with a variety of catalysts.

CATALYST DESCRIPTION

Loctite CAT 17 provides the following product characteristics:

  • High temperature resistant
  • Long work life
  • High temperature performance
  • Chemical resistant

Cure: Heat cure

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.23 g/cc0.0806 lb/in³Mixed
 2.40 g/cc0.0867 lb/in³Part A, Loctite Stycast 2762FT
Water Absorption 0.20 %
@Time 86400 sec
0.20 %
@Time 24.0 hour
Immersion
Brookfield Viscosity 150000 cP150000 cPMixed
 250000 cP250000 cPPart A, Loctite Stycast 2762FT
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9494
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Dielectric Constant 5.8
@Frequency 1e+6 Hz
5.8
@Frequency 1e+6 Hz
Dielectric Strength 15.0 kV/mm381 kV/in
Dissipation Factor 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 38.0 µm/m-°C21.1 µin/in-°F
Thermal Conductivity 1.34 W/m-K9.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 230 °C446 °F
Minimum Service Temperature, Air -20.0 °C-4.00 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  360 min
@Temperature 125 - 175 °C
6.00 hour
@Temperature 257 - 347 °F
Regular Castings: 3 hours @ 125°C plus 3 hours @ 175°C
 1680 min
@Temperature 65.0 - 150 °C
28.0 hour
@Temperature 149 - 302 °F
Large castings: 16 hrs @ 65°C, plus 6 hrs @ 125°C, plus 6 hrs @ 150°C
Working Life >= 1440 min
@Temperature 25.0 °C
>= 1440 min
@Temperature 77.0 °F
100 g
Shelf Life 12.0 Month12.0 MonthPart A, Loctite Stycast 2762FT
 
Descriptive Properties
AppearanceBlackPart A, Loctite Stycast 2762FT
Mix Ratio, by Weight100 : 10Material : Catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHENK7926 / 255413

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.