MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CLAL-MSX SICLANIC S® TF Quenched Copper Alloy, precipitation treated
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :
  • electrical conductivity greatly superior to that of bronzes, brasses and nickel silver
  • mechanicals properties on a par with those of copper cobalt- beryllium and of bronze
  • excellent fatigue strength
  • very competitive cost compared with copper-cobalt-beryllium.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.90 g/cc0.322 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 170 - 190170 - 190
 150
@Time 3600 sec
150
@Time 1.00 hour
 170
@Time 7200 sec
170
@Time 2.00 hour
 180
@Time 10800 sec
180
@Time 3.00 hour
 188
@Time 14400 sec
188
@Time 4.00 hour
 191
@Time 18000 sec
191
@Time 5.00 hour
Tensile Strength, Ultimate 580 - 680 MPa84100 - 98600 psi
Tensile Strength, Yield 450 - 550 MPa
@Strain 0.2 %
65300 - 79800 psi
@Strain 0.2 %
Elongation at Break 10 - 20 %10 - 20 %
Modulus of Elasticity 130 GPa18900 ksilongitudinal
Flexural Strength >= 430 MPa>= 62400 psiLimit of elasticity in Bending
Fatigue Strength 245 MPa
@# of Cycles 1.00e+7
35500 psi
@# of Cycles 1.00e+7
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000400 ohm-cm<= 0.00000400 ohm-cmprecipitation hardened
 0.00000430 ohm-cm0.00000430 ohm-cmprecipitation hardened (5 hr)
 0.00000440 ohm-cm0.00000440 ohm-cmprecipitation hardened (4 hr)
 0.00000460 ohm-cm0.00000460 ohm-cmprecipitation hardened (2 hr)
 0.00000460 ohm-cm0.00000460 ohm-cmprecipitation hardened (3 hr)
 0.00000490 ohm-cm0.00000490 ohm-cmprecipitation hardened (1 hr)
 0.00000780 ohm-cm0.00000780 ohm-cmquenched
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.6 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.370 J/g-°C0.0884 BTU/lb-°F
Thermal Conductivity 84.0 W/m-K583 BTU-in/hr-ft²-°Fsolid solution (or quenched) state
 188.4 W/m-K1307 BTU-in/hr-ft²-°Fquenched state
Melting Point 1040 - 1060 °C1900 - 1940 °F
Solidus 1040 °C1900 °F
Liquidus 1060 °C1940 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 96.9 %96.9 %
Nickel, Ni 2.5 %2.5 %
Silicon, Si 0.60 %0.60 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NCLAL096 / 160127

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.