MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Haysite H515 Polyester, High Temp Flex
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: H515 exhibits excellent flexibility and retention of electrical properties at elevated temperatures. For use in 220º C insulation systems in dry type transformers and where flexibility and high temperature is required. Standard color is tan. Thickness is 1/32" - 1/16". Sheet sizes are 36" x 72" and 48" x 96".

Information provided by Haysite

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D792
Water Absorption 1.1 %ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 6200 psiLW; ASTM D638
 6700 psiCW; ASTM D638
Compressive Strength 10800 psiFlatwise; ASTM D695
Izod Impact, Notched 9.00 ft-lb/inEdgewise (CW); ASTM D256
 10.0 ft-lb/inEdgewise (LW); ASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 5.2
@Frequency 60 Hz
ASTM D150
Dielectric Strength 560 V/milPerpendicular, short time in air; ASTM D149
 600 V/milPerpendicular, short time in oil; ASTM D149
Dissipation Factor 0.057
@Frequency 60 Hz
ASTM D150
Arc Resistance 135 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °CElec.
 200 °CMech.
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAY512 / 142468

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.