MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mitsubishi Iupiace® LN23 m-Polyphenylene Ether (m-PPE)
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: Flame retardant V-0 grade. Iupiace is a polymer alloy made by modifying PPE with high impact polystyrene (HIPS), nylon-6 or nylon-66. Usability in a wide range of temperatures (-40 to 160). Higher rigidity, impact strength and fatigue resistance. Excellent insulation properties, low dielectric constant and low dielectric dissipation factor. Excellent dimensional stability with low water absorption. Flame retardance and excellent self-extinguishing properties. Low density. Low shrinkage rate, ensuring quality precision parts. Good mold release, easy flow properties and a wide range of stock temperatures.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Water Absorption 0.070 %
@Temperature 23.0 °C
Immersion
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 300 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 47.0 MPaISO-527-1,2
Elongation at Break 25 %ISO 527-1,2
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 2400 MPaISO 178
Charpy Impact, Notched 11.0 kJ/m²ISO 179-1,2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+16 ohm-cmIEC 60093
Surface Resistance 2.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 55.0 µm/m-°CISO 11359-2
CTE, linear, Transverse to Flow 58.0 µm/m-°CISO 11359-2
Maximum Service Temperature, Air 160 °C
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °CISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75-1,2
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Iupiace® AH8P m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AP4 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® GN20 m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® LGX420N m-Polyphenylene Ether (m-PPE)
Mitsubishi Iupiace® AN70 m-Polyphenylene Ether (m-PPE)

PMITSU9122 / 191795

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.