MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kinetics MIM Ni as Sintered
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Most commonly used for applications requiring:
  • Electrical conductivity
  • Corrosion resistance.

Information provided by Kinetics, Inc.

Key Words: Metal Injection Molding
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.60 g/ccSintered Typical
 8.90 g/ccSintered Theoretical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000680 ohm-cmTheoretical
 0.00000930 ohm-cmTypical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PSM Industries PolyAlloys MIM-316L sintered Stainless Steel
Kinetics MIM 4605 Low Alloy Steel (Case Hardened)
Kinetics MIM 2.5% SiFe Soft Magnetic Steel
Kinetics MIM 17-4PH Stainless Steel (H900 Condition)
Kinetics MIM 4605 Low Alloy Steel (Austempered)

NKINET18 / 138097

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.