MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Unipetrol PE HD LITEN® FB/FL 20 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Made for tubular film and special applications.

Information provided by Unipetrol RPA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ISO 1183
ESCR 100% Igepal® >= 350 hour
@Temperature 50.0 °C
>= 350 hour
@Temperature 122 °F
ASTM D1693
Melt Flow  0.20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.20 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 22 g/10 min
@Load 2.16 kg,
Temperature 190 °C
22 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5656ISO 868
Tensile Strength, Yield 17.0 MPa2470 psiISO 527
Elongation at Yield 10 %10 %ISO 527
Flexural Modulus 0.600 GPa87.0 ksiISO 178
Charpy Impact, Notched  0.140 J/cm²
@Temperature 23.0 °C
0.666 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 114 °C237 °FISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
Ethydco Advancene™ EE-4010-AAH HDPE Pipe Extrusion
Bamberger Polymers Bapolene® 345F Medium Density Polyethylene, Film Extrusion Grade
LyondellBasell Alathon® M5370PX High Density Polyethylene, Extrusion Grade
LyondellBasell Alathon® H5618 High Density Polyethylene

PUNIP067 / 82927

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.