MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Copper Alloy, UNS C27400, Yellow Brass, 63%, OS025 Temper, Tube
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Nominal Grain Size 0.025 mm

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability –Gas Shielded Arc Welding, Capacity for Being Hot Formed

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Roll Threading and Knurling; Shearing; Spinning; Squeezing and Swaging; Stamping

Typical Uses: Cold Headed Parts; Plumbing Accessories; Plumbing Trap Tube; Traps

Applicable Specifications: Rod, Bar & Shapes - ASTM B927/B927M; Tube - ASTM B135, Seamless ASME SB135, Seamless (Metric) ASTM B135/B135M; Wire – ASTM B134/B134M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.44 g/cc0.305 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell F 8282
Tensile Strength 386 MPa56000 psi
Tensile Strength, Yield 159 MPa23000 psi0.5% Ext
Elongation at Break 50 %50 %
Tensile Modulus 103 GPa15000 ksi
Modulus of Rigidity 38.6 GPa5600 ksi
Poissons Ratio 0.340.34Calculated
Machinability 35 %35 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000620 ohm-cm0.00000620 ohm-cm27.6% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 20.5 µm/m-°C
@Temperature 20.0 - 300 °C
11.4 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 9.65 W/m-K67.0 BTU-in/hr-ft²-°F
Melting Point <= 916 °C<= 1680 °F
Liquidus 916 °C1680 °F
Annealing Point 427 - 704 °C800 - 1300 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 61 - 64 %61 - 64 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.090 %<= 0.090 %
Zinc, Zn 35.6 - 39 %35.6 - 39 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC27400x2 / 291840

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.