MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro DESMODUR®MTQ25130 + BAYTEC® T20 + BAYTEC® XL B + PLASTICIZER V04 (Catalyst CATD0812-3), 35 A Polyurethane, MDI- PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/ccBAYTEC® T20
 1.01 g/cc1.01 g/ccBAYTEC® XL B
 1.04 g/cc1.04 g/cc
 1.06 g/cc1.06 g/ccPLASTICIZER V04
 1.10 g/cc1.10 g/ccDESMODUR®MTQ25130
Viscosity 30 cP30 cPBAYTEC® XL B
 50 cP50 cPPLASTICIZER V04
 800 cP800 cPDESMODUR®MTQ25130
 1200 cP1200 cPBAYTEC® T20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3535DIN 53505
 29
@Temperature 80.0 °C
29
@Temperature 176 °F
DIN 53505
 40
@Temperature -5.00 °C
40
@Temperature 23.0 °F
DIN 53505
Tensile Strength at Break 18.0 MPa2610 psiDIN 53504
Tensile Stress at Strain 0.200 MPa
@Strain 10 %
29.0 psi
@Strain 10 %
DIN 53504
Elongation at Break 800 %800 %DIN 53504
100% Modulus 0.800 MPa
@Strain 100 %
116 psi
@Strain 100 %
DIN 53504
200% Modulus 1.10 MPa
@Strain 200 %
160 psi
@Strain 200 %
DIN 53504
300% Modulus 1.50 MPa
@Strain 300 %
218 psi
@Strain 300 %
DIN 53504
Resilience 6767[%]; DIN 53512
Tear Strength 9.00 kN/m51.4 pliwith nick; ISO 34-1
 27.0 kN/m154 pliwithout nick; ISO 34-1
Abrasion 6060[mm3]; ISO 4649
Compression Set 40 %
@Temperature 70.0 °C,
Time 79200 sec
40 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815-1
 
Processing PropertiesMetricEnglishComments
Processing Temperature 45.0 °C113 °FDESMODUR®MTQ25130
 45.0 °C113 °FBAYTEC® T20
 45.0 °C113 °FBAYTEC® XL B
 45.0 °C113 °FPLASTICIZER V04
Mold Temperature 100 °C212 °F
Pot Life 3.00 min3.00 min
 
Descriptive Properties
AppearanceliquidDESMODUR®MTQ25130
 liquidPLASTICIZER V04
 solidBAYTEC® T20
 solidBAYTEC® XL B
Content0.8CATD0812-3 % / total (by weight), (catalyst at the head)
 100Parts by weight of prepolymer
 12.9-13.3%NCO
 175Parts by weight of BAYTEC® T20
 200Parts by weight of PLASTICIZER V04
 5.87Parts by weight of BAYTEC® XL B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCOVEST0532 / 202315

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.