MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT SilSo Print 21001 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: Pourable, addition-curing, 2-part silicone rubber that cures at room temperature. This product is mainly used for making silicone printing pads. The cured rubber exhibits excellent physical and electrical properties. Fast and non-shrink cure at room temperature which can be accelerated considerably by the application of heat.

Key Features

  • The product can be diluted by adding silicone oil (50 – 300 mPas), which reduces the viscosity and hardness of the material.
  • Very good flow and detail reproduction properties due to low viscosity.
  • very good mechanical properties, even diluted.
  • Ink resistance.

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³A; BS ISO 2781
 1.10 g/cc0.0397 lb/in³B; BS ISO 2781
 1.10 g/cc0.0397 lb/in³Cured; BS ISO 2781
Brookfield Viscosity 8000 cP8000 cPB
 10000 cP10000 cPMixed
 12000 cP12000 cPA
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
Storage Temperature <= 30.0 °C<= 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3030DIN 53 505
Tensile Strength 6.998 MPa1015 psiDIN 53 504, S 3 A
Elongation at Break 600 %600 %DIN 53 504, S 3 A
Tear Strength 30.3 kN/m173 pliASTM D 624, Die B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 720 min12.0 hourDe-mould Time / Full Cure
Pot Life 30.0 min30.0 min
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancebrick-red
ColorwhiteA
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL156 / 314639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.