MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hostalen PP H2212 36 Polypropylene Blockcopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Hostalen PP H2212 36 is a polypropylene block copolymer grey colored similar to RAL 7032 (pebble grey) and is typically used by customers in the applications of compression molded sheets. The material Hostalen PP H2212 36 is not intended for medical and pharmaceutical applications.

Availability: Europe

Application: Industrial; Plumbing, Heating & Cooling

Market: Industrial, Building & Construction; Pipe

Processing Method: Compression Molding; Injection Molding; Pipe

Attribute: Block Copolymer

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.908 g/ccISO 1183-1
Melt Flow 0.450 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 1.20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133-1
 2.10 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57.0ISO 868
Ball Indentation Hardness 30.0 MPaH 132/30; ISO 2039-1
Tensile Strength, Yield 24.0 MPaISO 527-1, -2
Elongation at Break 26.0 %50 mm/min; ISO 527-1, -2
Tensile Modulus 800 MPaISO 527-1, -2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CUnannealed; ISO 75B-1, -2
Vicat Softening Point 61.0 °CB50; ISO 306
 150 °CA50; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9627 / 324562

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.