MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Avient Synprene® IT38-004M Thermoplastic Elastomer - SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Description/Features:
  • High Performance Thermoplastic Elastomer
  • Natural
  • Over-Molding Grade
  • Transparent

Applications:

  • Multi-Purpose

Market:

  • Consumer Goods

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Linear Mold Shrinkage 0.026 cm/cm0.026 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 3636Instant; ASTM D2240
Tensile Strength at Break 5.38 MPa780 psiMethod A (Dumbbell & Section), 20 in/min; ASTM D412
Tensile Stress at Strain 2.28 MPa
@Strain 300 %
330 psi
@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 700 %700 %Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 21.9 kN/m125 pliDie C (graves), 20 in/min; ASTM D624
Compression Set 21 %
@Temperature 23.0 °C,
Time 79200 sec
21 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; ASTM D395
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %transparent; thickness not quantified

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade
Avient Synprene® ST-6130 Thermoplastic Elastomer - SBC
Avient Synprene® ST-6120 Thermoplastic Elastomer - SBC
Avient Synprene® ST-6110 Thermoplastic Elastomer - SBC
Avient Synprene® RT-3840MS Thermoplastic Elastomer - SBC

PH1PO3222 / 44953

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.