MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Angst+Pfister APSOplast® PTFE 500 PTFE + mica
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: This grade is subject to nine times less deformation under load than unfilled PTFE (tested as per ASTM D 621; compressive stress of 14 MPa at 50 °C). Its coefficient of linear thermal expansion approaches the elongation rate of aluminium and is five times that of unfilled PTFE. PTFE 500 is considerably harder than unfilled PTFE but – at practically the same coefficient of friction – has improved wear resistance and does not attack most mating partners.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.30 g/cc0.0831 lb/in³DIN EN ISO 1183-1
Water Absorption at Saturation 0.10 %0.10 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 8.00 MPa1160 psiDIN EN ISO 527
Elongation at Break 10 %10 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 2.20 GPa319 ksiDIN EN ISO 527
Compressive Strength 17.0 MPa
@Strain 1 %
2470 psi
@Strain 1 %
ISO 604
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179-1/1eU
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+13 ohm-cm>= 1.00e+13 ohm-cmDIN IEC 60023
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmANSI/ESD STM 11.11
Dielectric Constant 2.85
@Frequency 1e+6 Hz
2.85
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 11.0 kV/mm279 kV/in
Dielectric Loss Index 0.0080
@Frequency 1e+6 Hz
0.0080
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 50.0 µm/m-°C
@Temperature 23.0 - 95.0 °C
27.8 µin/in-°F
@Temperature 73.4 - 203 °F
ASTM D 696
Thermal Conductivity 0.770 W/m-K5.34 BTU-in/hr-ft²-°FDIN 52612-1
Melting Point 327 °C621 °F
Maximum Service Temperature, Air 260 °C500 °Flong term
 280 °C536 °Fshort term
Minimum Service Temperature, Air -20.0 °C-4.00 °F
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Descriptive Properties
Colorivory

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PANGP081 / 250579

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.