MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® HP4000 Pipe HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: High Density Hexene Copolymer

Formolene® HP4000 is a high performance copolymer that is designed for the most demanding requirements of non pressure pipe applications. It has good long-term hoop strength performance, very high melt strength, and outstanding toughness even at low temperatures. Formolene® HP4000 meets all requirements of ASTM D4976 – PE 235. Formolene® HP4000 meets the requirements of ASTM F 2160 for use in solid wall HDPE conduit based pipe.

Applications: Telecommunications Conduit and Non-Pressure Pipe Applications

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccASTM D1505
ESCR 100% Igepal® >= 1000 hourCondition A, B, C, F50; ASTM D1693
Melt Flow 0.16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Condition E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 5000 psi2" (50mm) per min, Type IV; ASTM D638
Tensile Strength, Yield 3200 psi2" (50mm) per min, Type IV; ASTM D638
Elongation at Break >= 500 %2" (50mm) per min, Type IV; ASTM D638
Flexural Modulus 110000 psiASTM D3350
 140000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -90.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethydco Advancene™ EE-4010-AAH HDPE Pipe Extrusion
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin

PFPCPQ057 / 150289

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.