System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Sichuan Deyang Haton® hp23310 Polyphenylene Sulfide Coating
Categories:
Polymer
;
Thermoplastic
;
Polyphenylene Sulfide (PPS)
;
Polyphenylene Sulfide (PPS) Coating Resin
Material Notes:
Powder; anti-corrosion, wear resistant
Information provided by Sichuan Deyang Chemical Co., LTD
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Water Absorption
<= 0.030 %
GB/T 1034-2008
Mechanical Properties
Original Value
Comments
Impact
NB
Gb1720
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
160
-
220
°C
Descriptive Properties
Chemical Resistance
Ammonia, 40%
< 0.001 mg/h*cm
2
Hydrochloric Acid, 40%
< 0.001 mg/h*cm
2
Sodium Chloride, 5%
< 0.001 mg/h*cm
2
Sodium Hydroxide, 50%
< 0.001 mg/h*cm
2
Sulfuric Acid, 40%
< 0.001 mg/h*cm
2
Pencil Hardness
>2 H
GB/T6739
Wear Resistance, g
= 0.029
GB1768-79
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Sichuan Deyang Haton® hs2331B Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hs23310 Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hs1237B Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hs12370 Polyphenylene Sulfide Coating
Sichuan Deyang Haton® hp12370 Polyphenylene Sulfide Coating
PSICHU934 / 156175
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.