MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plenco 50335 PET, Pellet, Injection Molded, White  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.

Information supplied by Plenco


Plenco discontinued their PET product line in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.64 g/ccASTM D792
Water Absorption 0.050 %ASTM D570
Linear Mold Shrinkage 0.0018 cm/cmATM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 120.5 MPaASTM D638
Elongation at Break 1.81 %ASTM D638
Tensile Modulus 9.47 GPaASTM D638
Flexural Yield Strength 179.3 MPaASTM D790
Flexural Modulus 9.04 GPaASTM D790
Compressive Yield Strength 172.7 MPaASTM D695
Izod Impact, Notched 0.560 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 3.96e+17 ohm-cmASTM D257
Dielectric Constant 3.5
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.3 kV/mmShort Time; ASTM D149
Dissipation Factor 0.013
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 70 secASTM D495
Comparative Tracking Index 250 VASTM D3638
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 224 °CHeat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 218 °CASTM D648
Flammability, UL94 HB
@Thickness 1.47 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC407 Non-Reinforced
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant
BASF Ultradur® B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET

PLEM74 / 50762

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.