MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Zytel® RS LC3160 NC010 PA610  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610)

Material Notes:

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccDAM; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPaDAM; ISO 527-1/-2
Elongation at Break >= 50 %DAM; ISO 527-1/-2
Elongation at Yield 3.5 %DAM; ISO 527-1/-2
Tensile Modulus 2140 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.39DAM; ISO 527-1/-2
Charpy Impact, Notched 6.00 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 225 - 235 °CExtrusion
 230 °CExtrusion Optimum
Drying Temperature 75.0 °CExtrusion
 80.0 °CExtrusion
Dry Time 3.00 - 4.00 hourDehumidified Dryer; Extrusion
Moisture Content 0.060 %Extrusion
 
Descriptive Properties
Delivery formPellets
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>PA610<ISO 11469
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Resin IdentificationPA610ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® RS LC3090 NC010 PA610
Celanese Zytel® RS LC3060 NC010 PA6.10
Multibase TPSiV® 4200-80A Thermoplastic Silicone Vulcanizate
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced

PZDSX5499 / 198139

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.