MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

RAUH Polymers PermaFlex® 55 COPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: PermaFlex®, and all its grades, is a thermoplastic elastomer, based on copolyester chemistry, also known as COPE or TPE-E. It eliminates the demarcation between rubbers and engineering plastics. It combines the strength and processing characteristics of engineering plastics with the performance of thermoset elastomers, a combination of the most desirable characteristics of rubbers and plastics. This combination provides benefits in processing and productivity for both molders and extruders. It also can be processed by blow molding or rotational techniques. As a thermoplastic, PermaFlex does not involve the high cost of vulcanization to obtain optimal properties. This polyester-based material offers a consistent performance over its entire operating temperature range, since its properties vary minimally from high to low temperature extremes. PermaFlex polyester-ester technology extends the traditional temperature range of thermoplastic elastomers.

Basic Properties: A wide range of properties can be created by varying the ratio of soft to hard block and the composition of the soft segment. PermaFlex stays tough as it flexes and recovers, having excellent characteristics as follows:

  • Temperature resistance
  • High tensile strength
  • Impact resistance
  • Wear and tear
  • Abrasion resistance
  • Resistance to weathering, oil and chemicals
  • High permeability resistance to fuels and oils
  • Flexural fatigue endurance
  • UV stability
  • Adhesion compatibility with paints, glues, plastics and metals
  • Creep and compression resistance
  • Excellent moisture vapor transmission rate
  • Dielectric
  • Good tactile and soft touch feel

Information provided by Rauh Polymers Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ASTM D792
Linear Mold Shrinkage 0.0127 - 0.0152 cm/cm0.0127 - 0.0152 in/inType 1 Bar
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm0.0050 - 0.0060 in/inASTM D955
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 240 °C
50 g/10 min
@Load 4.76 lb,
Temperature 464 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ASTM D2240
Tensile Strength at Break  48.3 MPa
@Temperature -40.0 °C
7000 psi
@Temperature -40.0 °F
Type 1 Bar; ASTM D638
 48.3 MPa
@Temperature 23.0 °C
7000 psi
@Temperature 73.4 °F
Type 1 Bar; ASTM D638
Elongation at Break  900 %
@Temperature -40.0 °C
900 %
@Temperature -40.0 °F
Type 1 Bar; ASTM D638
 900 %
@Temperature 23.0 °C
900 %
@Temperature 73.4 °F
Type 1 Bar; ASTM D638
Izod Impact, Notched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
For Impact Modified Version; ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Dart Drop, Total Energy >= 434 J>= 320 ft-lb
Taber Abrasion, mg/1000 Cycles 30.8930.89H-18, 1000 gm; ASTM D3389
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C425 °F
Vicat Softening Point 204 °C399 °FRate A; ASTM D648
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Grades available
 
Processing PropertiesMetricEnglishComments
Processing Temperature 199 - 271 °C390 - 520 °F
Rear Barrel Temperature 204 - 210 °C400 - 410 °F
Middle Barrel Temperature 227 - 232 °C440 - 450 °F
Front Barrel Temperature 227 - 232 °C440 - 450 °F
Nozzle Temperature 232 - 238 °C450 - 460 °F
Melt Temperature 232 - 266 °C450 - 510 °F
Mold Temperature 54.4 - 65.6 °C130 - 150 °F
Drying Temperature 77.0 - 82.0 °C171 - 180 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourto achieve .02% Moisture
Injection Pressure 82.7 - 89.6 MPa12000 - 13000 psi
Hold Pressure 68.9 - 75.8 MPa10000 - 11000 psi
Back Pressure 0.000 - 2.76 MPa0.000 - 400 psi
 
Descriptive Properties
Tear Resistance[20 in/min], ASTM D624 Die C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAUH002 / 296462

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.