MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ametek 17-4 P/M Process, Sintered at 2300°F (1260°C)
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: Composition reported is typical of 17-4 precipitation hardening stainless. This alloy is widely used because of its high strength, high hardness, excellent corrosion resistance, and easy heat treatment. The 17-4 PH alloy is used in aerospace, medical, food processing, and chemical industries for applications such as pump shafts, valve stems, braces, fasteners, coupling, rocket and missile components, hydraulic actuators, and wear rings.

Mechanical property data below is from samples aged for 1 hour at 900°F (482°C) in hydrogen - the H900 condition, which maximizes strength. The properties that can be expected for material that was lubricated with 3/4% Acrawax C and compacted at 48 tsi are shown below.

17-4 PH is a registered trademark of Armco, Inc.; information provided by Ametek Specialty Metal Product Division.

Key Words: UNS S17400, Powder metallurgy, 17-4PH, 17/4PH, 17-4 PH, 17/4 PH, Precipitation Hardening
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 105
Tensile Strength, Ultimate 900 MPa
Tensile Strength, Yield 660 MPa
Elongation at Break 1.8 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.035 %
Chromium, Cr 16.3 %
Copper, Cu 4.0 %
Iron, Fe 74 %as balance
Manganese, Mn 0.50 %
Nickel, Ni 4.0 %
Niobium, Nb (Columbium, Cb) 0.30 %
Phosphorus, P 0.020 %
Silicon, Si 0.50 %
Sulfur, S 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ametek 17-4 P/M Process, Sintered at 2200°F (1204°C)
Kinetics MIM 17-4PH Stainless Steel (As Sintered)
Ametek 17-4 P/M Process, Sintered at 2050°F (1121°C)
FloMet 17-4 PH Stainless Steel, As Sintered
Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)

NMA152 / 18159

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.