MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites LYTEX® 4129 63% Glass Fiber Reinforced Epoxy SMC
Categories: Polymer; Thermoset; Composite SMC; Epoxy; Epoxy/Glass SMC

Material Notes: LYTEX 4129 is an epoxy high performance, glass fiber reinforced ESC molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and excellent electrical properties.

  • Form = Sheet
  • Color = Black
  • Glass Fiber Content = 63% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/ccASTM D792
Water Absorption 0.070 %ASTM D570
Linear Mold Shrinkage 0.0010 in/inASTM D955
Spiral Flow 20.0 in
@Pressure 27.6 MPa,
Temperature 163 °C
Mesa
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 262 MPaASTM D638
Flexural Strength 440 MPaASTM D790
Flexural Modulus 16.5 GPaASTM D790
Izod Impact, Notched 1869 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+14 ohm-cmASTM D257
Dielectric Constant 4.3
@Frequency 100 Hz
ASTM D150
Dielectric Strength 500 V/milASTM D149
Dissipation Factor 0.0080
@Frequency 100 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °CDeflection Temperature, Load not specified; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 330 °FMold Temperature
Cure Time 5.00 - 10.0 min
Shelf Life 6.00 Month
@Temperature -17.8 °C
 
Descriptive Properties
Fiber Length (in)0.5Glass, nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4084 63% Glass Fiber Reinforced Epoxy SMC
Quantum Composites Lytex® 4149 55% Carbon Fiber Epoxy SMC
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND F110 Epoxy Adhesive
BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer

PCOQB913 / 139281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.