MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UNS C87610, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes: Applications: bearings, belts, Impellers, pump and valve components, marine fittings, corrosion-resistant casting.

<>Typical data for as-sand-cast separately cast test bars (M01 temper).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 85500 kg, typical
Tensile Strength, Ultimate 380 MPa
Tensile Strength, Yield 170 MPa
@Strain 0.5 %
Elongation at Break 30 %in 50 mm
Modulus of Elasticity 105 GPa
Compressive Strength 125 MPaat 0.001 mm/mm set
 415 MPaat 0.01 mm/mm
Machinability 40 %UNS C36000 (free-cutting brass) = 100%
Shear Strength 193 MPaTypical
Izod Impact 45.0 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000028735 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 16.4 BTU-in/hr-ft²-°F
Melting Point 1510 - 1780 °F
Solidus 1510 °F
Liquidus 1780 °F
Shrinkage 2.1 %Patternmaker's Shrinkage (1/4 in./ft.)
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 260 °CStress-Relieving Temperature
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu >= 90 %
Iron, Fe <= 0.20 %
Lead, Pb <= 0.20 %
Manganese, Mn <= 0.25 %
Other, total <= 0.50 %
Silicon, Si 3.0 - 5.0 %
Zinc, Zn 3.0 - 5.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Everdur, UNS C87300, Copper Casting Alloy
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
Low-Zinc Silicon Brass, UNS C87600, Copper Casting Alloy
MetalTek NAVY G Cast UNS C90300 Bearing Bronze
UNS C83400, Copper Casting Alloy

MC87610b1 / 11923

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.