MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Kraton® D1116 A (SBS) Radial Triblock Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1116 A is a clear, radial triblock copolymer based on styrene and butadiene with a polystyrene content of 23%. It is supplied from Europe in the physical form identified:
Kraton D1116 AT - supplied as a porous pellet dusted with talc
Kraton D1116 ASM - supplied as a powder dusted with silica
Kraton D1116 A IM - supplied as a powder dusted with inorganic dusting agents for supply to the North American market

Region: Asia Pacific, Europe, Japan, North America, and South America

Uses: Kraton D1116 A is used as a modifier of bitumen and polymers. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants, and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccISO 2781
Volatiles <= 0.30 %<= 0.30 %KM 04
Viscosity 2000 - 3000 cP2000 - 3000 cP25% Toluene Solution at 25°C; KM 06
Ash <= 0.35 %<= 0.35 %AT; ISO 247
 2.5 - 4.5 %2.5 - 4.5 %AIM; BAM 908
 2.5 - 5.0 %2.5 - 5.0 %ASM; ISO 247
 
Descriptive Properties
ContentAntioxidant>0.14%, KM 08
 Polystyrene21.5-24.1%, KM 03
 Total Extractables<1.0%, KM 05

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® FG1901 + PBT blend (30/70)
Kraton® D1102 B (SBS) Liner Block Copolymer
Kraton® D1101 E (SBS) Liner Block Copolymer
Kraton® D1102 J (SBS) Liner Block Copolymer
Kraton® D1102 E (SBS) Liner Block Copolymer

PKRA9813 / 132712

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.