MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mallard Creek Polymers Rovene® 4848 Non-Carboxylated Styrene-Butadiene Emulsion
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: ROVENE® 4848 is a new developmental polymer specifically designed to be used in two part spray adhesives for open or closed cell foams and other contact and cold seal applications. Fast breaking characteristics may allow its use in specially formulated one part spray adhesives. When working with ROVENE® 4848 it is important to remember that it may be tackified, thickened, and blended with other carboxylated and non-carboxylated emulsions. It may also be blended with polychloroprene and natural latex if properly formulated. This flexibility allows for the formulating of a wide variety of adhesives with custom performance properties.
APPLICATION: ROVENE® 4848 has found applications in two part foam-to-foam, one and two part fast breaking spray up adhesives, and special contact or cold seal applications in combination with polychloroprene and natural latex.

Information provided by Mallard Creek Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 52 - 54 %
Particle Size 0.17 µm
pH 11 - 12
Brookfield Viscosity 200 - 800 cP#2/20 rpm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 40 %
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -38.0 °C
 
Descriptive Properties
EmulsifiersRosin Acid Soap

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mallard Creek Polymers Rovene® 8001 Carboxylated Styrene-Butadiene Emulsion
Mallard Creek Polymers Rovene® 5499 Carboxylated Styrene-Butadiene Emulsion
Mallard Creek Polymers Rovene® 4201 Carboxylated Styrene-Butadiene Emulsion
Colorite Polymers Flexchem 4051-02 Vinyl Compound
Colorite Polymers 7077 Non-Phthalate 77 Series Vinyl Compound

PMCP057 / 104714

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.