MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Copper Alloy, UNS C40810, H08 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Spring

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Butt Weld; Fair Suitability – Capacity for Being Hot Formed

Typical Uses: Terminals, automotive; Connectors, electronic; Contact springs; Lead Frames

Applicable Specifications: Bar – ASTM B591; Strip – ASTM B888/B88M, ASTM B591

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 662 MPa96000 psi
Tensile Strength, Yield 641 MPa93000 psi0.2% Offset
Elongation at Break 3.0 %3.0 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 41.4 GPa6000 ksi
Poissons Ratio 0.420.42Calculated
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000520 ohm-cm0.00000520 ohm-cm33% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.2 µm/m-°C
@Temperature 20.0 - 300 °C
10.1 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 11.8 W/m-K82.0 BTU-in/hr-ft²-°F
Melting Point 1035 - 1050 °C1895 - 1930 °F
Solidus 1035 °C1895 °F
Liquidus 1050 °C1930 °F
Annealing Point 349 - 732 °C660 - 1350 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 94.5 - 96.5 %94.5 - 96.5 %
Iron, Fe 0.080 - 0.12 %0.080 - 0.12 %
Lead, Pb <= 0.050 %<= 0.050 %
Nickel, Ni 0.11 - 0.20 %0.11 - 0.20 %
Phosphorus, P 0.028 - 0.040 %0.028 - 0.040 %
Tin, Sn 1.8 - 2.2 %1.8 - 2.2 %
Zinc, Zn 1.0 - 3.5 %1.0 - 3.5 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC40810x6 / 291884

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.