MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Axiall 7751 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 7751 is a vertical blind profile exterior compound requiring the following properties:
  • Impact Strength & Toughness
  • Colorability
  • Dimensional Stability
  • UV Color Stability
  • Easy Processing in Thin Parts at Fast Rates

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111.9111.9ASTM D-785
Hardness, Shore D 8181ASTM D-2240
Tensile Strength, Yield 40.5 MPa5870 psiASTM D-638
Tensile Modulus 3.22 GPa467 ksiASTM D-638
Flexural Strength 74.19 MPa10760 psiASTM D-790
Flexural Modulus 3.07 GPa445 ksiASTM D-790
Izod Impact, Notched  1.44 J/cm
@Thickness 6.35 mm
2.70 ft-lb/in
@Thickness 0.250 in
ASTM D-256
 2.14 J/cm
@Thickness 3.17 mm
4.00 ft-lb/in
@Thickness 0.125 in
ASTM D-256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 69.50 °C157.1 °FASTM D-648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGGUL418 / 41694

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.