MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Poly-Pale™ Partially Dimerized Rosin
Categories: Polymer

Material Notes: Product Description: Poly-Pale™ resin is a pale, partially polymerized (dimerized) rosin. Compared with pale grades of regular wood, gum, or tall oil rosins, it has a higher softening point, higher viscosity (molten and in solution), much greater resistance to oxidation, and complete freedom from crystallizing when in solid form or in solution. Its many uses include the preparation of varnishes, driers, synthetic resins, ink vehicles, floor tile, rubber compounds, solder fluxes, and various adhesives and protective coatings.

Application/Uses:

  • Assembly
  • Bookbinding
  • Caulks and Sealants
  • Contact Adhesives
  • Footwear and Leather
  • Hot Melt Adhesives
  • Laminating
  • Nonwovens
  • Packaging
  • Pressure sensitive adhesives
  • Solventborne Adhesives
  • Tapes and Labels
  • Wax Modification
  • Wire and Cable
Key Attributes:
  • Alcohol-soluble
  • High softening point
  • Non-crystalline
  • Resistant to oxidation
  • Thermoplastic rosin acid

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.069 g/cc
Brookfield Viscosity 33 cP
@Temperature 180 °C
Melt, Thermosel
 100 cP
@Temperature 160 °C
Melt, Thermosel
 400 cP
@Temperature 140 °C
Melt, Thermosel
 4100 cP
@Temperature 120 °C
Melt, Thermosel
 100800 cP
@Temperature 100 °C
Melt, Thermosel
Molecular Weight 313 g/molMn
 353 g/molMw. Mw/Mn ratio = 1.13
 422 g/molMz
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 155[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 103 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 8.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5537 / 222731

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.