MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total 4320WZ Polypropylene, Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4320WZ is a nucleated impact copolymer. 4320WZ is characterized by good stiffness and remarkable impact resistance coupled with high creep resistance. This grade has been developed for injection molding of chair shells, pails, crates and other articles requiring good mechanical properties.

Application

Applications of ATOFINA 4320WZ has been specially formulated with an additive for excellent antistatic properties as well as good surface appearance and mold release.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 3.5 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3700 psiASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 190000 psiASTM D 790
Izod Impact, Notched 275 J/mASTM D256
 55.0 J/m
@Temperature -20.0 °C
ASTM D256
Charpy Impact Unnotched >= 3.00 J/cm²ASTM DIN53453
 0.900 J/cm²
@Temperature -20.0 °C
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CASTM D648
Vicat Softening Point 150 °CASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene HP0335T40V Homopolymer Talc Reinforced
TIMCAL TIMREX® PP 25 Natural Flake Graphite
Aclo Accuguard Polypropylene CP0467V0CSV Copolymer Flame Retardant Automotive Approved grade
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized
Aclo Accucomp Polypropylene HPO309L Homopolymer

PFINAA067 / 38503

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.