MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Therminol VP-1 Heat Transfer Fluid
Categories: Fluid

Material Notes: Therminol VP-1 heat transfer fluid is an ultra-high temperature synthetic heat transfer fluid designed to meet the demanding requirements of vapor phase systems or liquid phase systems.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
@Temperature 25.0 °C
Liquid; ASTM D4052
 1.068 g/cc
@Temperature 15.0 °C
Liquid; ASTM D4052
Kinematic Viscosity at 40°C (104°F) 0.248 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 0.99 cStASTM D445
Molecular Weight 166 g/mol
Surface Tension 36.6 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.20[mg KOH/g]; ASTM D664
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.35ASTM D924
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 206 J/gat max. use temperature
CTE, linear 97.9 µm/m-°C
@Temperature 200 °C
Crystallization Temperature 12.0 °C
Boiling Point 257 °C
Flash Point 110 °CPMCC; ASTM D93
 124 °CCOC; ASTM D92
 
Descriptive Properties
AppearanceClear, water white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5625 / 222819

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.