MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Ixef® 5002 Polyarylamide (PARA), 20% Glass\PTFE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyarylamide (PAA); Polyarylamide, Glass Fiber Filled

Material Notes: Ixef 5002 is a 20% glass-fiber reinforced, PTFE modified polyarylamide which exhibits very good mechanical performance, very good surface gloss, and superior wear properties.

- Natural: Ixef 5002/0085
- Custom Colorable

Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Wear Resistance; High Flow; High Stiffness; High Strength; Low Friction; Low Moisture Absorption; Outstanding Surface Finish

Uses: Appliance Components; Appliances; Automotive Applications; Automotive Electronics; Bushings; Business Equipment; Cams; Cell Phones; Electrical Housing; Electrical/Electronic Applications; Furniture; Gears; Industrial Applications; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools

Availability: Africa & Middle East; Asia Pacific; Europe; North America; South America

Hot Runners: 250°C to 260°C (482°F to 500°F)
Injection Pressure: rapid

Drying
The material as supplied is ready for molding without drying. However, If the bags have been open for longer than 24 hours, the material needs to be dried. When using a desiccant air dryer with dew point of -28°C (-18°F) or lower, these guidelines can be followed: 0.5-1.5 hour at 120°C (248°F), 1-3 hours at 100°C (212°F), or 1-7 hours at 80°C (176°F).

Injection Molding
IXEF 5002 compound can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The measured melt temperature should be about 280°C (536°F), and the barrel temperatures should be around 250°C to 260°C (482°F to 500°F) in the rear zone, gradually increasing to 260°C to 290°C (500°F to 554°F) in the front zone. If hot runners are used, they should be set to 250°C to 260°C (482°F to 500°F).

To maximize crystallinity, the temperature of the mold cavity surface must be held between 120°C and 140°C (248°F and 284°F). Molding at lower temperatures will produce articles that may warp, have poor surface appearance, and have a greater tendency to creep. Set injection pressure to give rapid injection. Adjust holding pressure and hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled (95%-99%).

Information provide by Solvay Specialty Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccISO 1183
Water Absorption 0.22 %24 hrs; ISO 62
Linear Mold Shrinkage 0.0020 - 0.0040 in/inISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 135 MPaISO 527-2
Elongation at Break 2.2 %ISO 527-2
Tensile Modulus 10000 MPaISO 527-2
Flexural Strength 215 MPaISO 178
Flexural Modulus 8000 MPaISO 178
Izod Impact, Notched 60.0 J/mASTM D256
Izod Impact, Unnotched 3.70 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Dielectric Constant 3.9
@Frequency 110 Hz
IEC 60250
Dielectric Strength 28.0 kV/mmIEC 60243-1
Dissipation Factor 0.015
@Frequency 110 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 29.0 µm/m-°CISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 220 °CUnannealed; ISO 75-2/A
Oxygen Index 23 %ISO 4598-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 250 - 260 °C
Front Barrel Temperature 260 - 290 °C
Melt Temperature 280 °C
Mold Temperature 120 - 140 °C
Drying Temperature 120 °C
Dry Time 0.500 - 1.50 hour
 
Descriptive Properties
Additional PropertiesMoisture Absorption - Internal Method: 1.8 %
AppearanceColors Available; Natural Color
FormsPellets
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 209 K TFE 15 Polyarylamide (PAA), Glass Fiber - PTFE Lubricated
RTP Company RTP 203 K TFE 15 Polyarylamide (PAA), Glass Fiber - PTFE Lubricated
Celanese VECTRA S135 LCP, 35% Glass Reinforced
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced
Celanese VECTRA S471 LCP, 45% Mineral / Glass Reinforced

PSOLVAY155 / 122453

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.