MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID 66 GF 50 HTS PA 66 reinforced with 50% glass fibre, with hydrolysis and thermal stabilization
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Features: PA 66 for injection moulding, chemically reinforced with 50% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delivered in black colour.

Packaging, transport, stocking: The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: Polyamide 66 (PA66)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/cc
Linear Mold Shrinkage 0.0047 cm/cm
Linear Mold Shrinkage, Transverse 0.0066 cm/cm
Melt Flow 5.0 g/10 min
@Load 0.325 kg,
Temperature 275 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 235 MPa
Elongation at Break 2.0 %
Tensile Modulus 17000 MPa
Flexural Strength 240 MPa
Flexural Modulus 13500 MPa
Charpy Impact Unnotched 100 kJ/m²
@Temperature 23.0 °C
 100 kJ/m²
@Temperature -20.0 °C
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -20.0 °C
 20.0 kJ/m²
@Temperature 23.0 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Strength 40.0 kV/mm
Comparative Tracking Index 400 V
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
Vicat Softening Point 250 °C
Flammability Test 1.0
Glow Wire Test 650 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 320 °C
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Moisture Content 0.15 %
Injection Pressure 70.0 - 120 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 50 Polyamide 66, 50% Glass Fiber
Celanese Zytel® ST801AHS BK010 PA66-HI
Plastcom SLOVAMID 66 GF 50 TS PA 66 reinforced with 50% glass fibre, thermal stability
Akro-Plastic Akromid® A3 GF 50 black PA 6.6 Conditioned, 50% Glass Filled
Celanese SO.F.TER Nivionplast® BR50G PA66 compound, 50% GF

PPLACO523 / 122724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.