MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® 840B Nylon 66, Extrusion Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded; Nylon 66, Film

Material Notes: 840B is a PA66-based copolymer that features high melt strength with ideal shear thinning behavior, high tensile strength, ductility, and clarity making it ideal for blown and cast film applications. Having a melt temperature between PA6 and PA66, it is a preferred material of choice compared to physical blends of PA6 and PA66 due to the ability to process at lower temperatures and produce a homogenous film resulting in uniform melting behavior, high gloss, and clarity. Further, 840B also allows for improved process flexibility due to its slower crystallization rate versus PA66 homopolymers giving a film processor higher potential blow up ratios and the ability for post-processes such as thermoforming and orienting.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.674 g/cc0.0243 lb/in³ASTM D1895
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %ASTM D6869
Viscosity Measurement 3.8 - 4.13.8 - 4.1Relative Viscosity - Sulfuric Acid; ISO 307
 115 - 145115 - 145Relative Viscosity - Formic Acid; ASTM D789
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance >= 2400 N
@Thickness 0.0250 mm
>= 540 lb (f)
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM F1306
Film Tensile Strength at Yield, MD 31.0 MPa
@Thickness 0.0380 mm
4500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Yield, TD 31.0 MPa
@Thickness 0.0380 mm
4500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Tensile Strength, Yield 78.0 MPa11300 psiDry; ISO 527-2
Film Elongation at Break, MD  120 %
@Thickness 0.0250 mm
120 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 390 %
@Thickness 0.0380 mm
390 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Break, TD  110 %
@Thickness 0.0250 mm
110 %
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 480 %
@Thickness 0.0380 mm
480 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, MD 6.5 %
@Thickness 0.0380 mm
6.5 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Film Elongation at Yield, TD 6.4 %
@Thickness 0.0380 mm
6.4 %
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
Elongation at Break 170 %170 %Dry; ISO 527-2
Flexural Strength 84.0 MPa12200 psiDry; ISO 178
Secant Modulus, MD  0.601 GPa
@Thickness 0.0380 mm
87.2 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 3.31 GPa
@Thickness 0.0250 mm
480 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Secant Modulus, TD  0.558 GPa
@Thickness 0.0380 mm
80.9 ksi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 3.31 GPa
@Thickness 0.0250 mm
480 ksi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Dry; ISO 180
Elmendorf Tear Strength MD 51.1 g
@Thickness 0.0380 mm
51.1 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Elmendorf Tear Strength TD 109 g
@Thickness 0.0380 mm
109 g
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1922
Dart Drop Test >= 2000 g
@Thickness 0.0380 mm
>= 4.41 lb
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D1709A
Film Tensile Strength at Break, MD  121 MPa
@Thickness 0.0380 mm
17500 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 280 MPa
@Thickness 0.0250 mm
40600 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
Film Tensile Strength at Break, TD  101 MPa
@Thickness 0.0380 mm
14600 psi
@Thickness 0.00150 in
Cast Film, Conditioned; ASTM D882
 280 MPa
@Thickness 0.0250 mm
40600 psi
@Thickness 0.000984 in
Cast Film, Conditioned; ASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 244 °C471 °FISO 11357-3
Crystallization Temperature 185 - 195 °C365 - 383 °FISO 11357-3
Shrinkage, MD 0.90 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
0.90 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
Shrinkage, TD 0.80 %
@Treatment Temp. 160 °C,
Thickness 0.0250 mm
0.80 %
@Treatment Temp. 320 °F,
Thickness 0.000984 in
Cast Film, Conditioned; ASTM D1204
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 60.0 °C68.0 - 140 °FBlow Film Air Temperature
 265 - 285 °C509 - 545 °FCylinder - Extrusion
Die Temperature 270 - 295 °C518 - 563 °FExtrusion
 70.0 - 80.0 °C
@Time 0.000 - 14400 sec
158 - 176 °F
@Time 0.000 - 4.00 hour
Extrusion
Melt Temperature 244 °C471 °FExtrusion
Moisture Content 0.030 - 0.080 %0.030 - 0.080 %Extrusion
 
Compliance PropertiesMetricEnglishComments
European Food 1935/2004 YesYes
FDA YesYes21CFR 177.1500
 
Descriptive Properties
Agency RatingsEU 10/2011
 EU 2023/2006
FeaturesGood Chemical Resistance
 Good melt strength
 High Melt Stability
 High Strength
 High Toughness/elongation
 Puncture resistant
Melt Pressure MPa3-17
Processing MethodCast Film
 Extrusion
 Profile extrusion
Screw DesignGP or Barrier
UsesIndustrial Applications
 Monofilaments
 Multilayer film
 Profiles
 Rods
 Sheet
 Tubing
 Vacuum Bagging Film

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Kynar® Film 302 PGM TR PVDF
Arkema Kynar® Film 252 PGM TR PVDF
Ascend Performance Materials Vydyne® 75HB NT0679 Nylon 66, Extrusion Grade
Ascend Performance Materials Vydyne® 75HB NT0679 Nylon 66 Compounding Grade
Ascend Performance Materials Vydyne® 833C Nylon 66, Extrusion Grade

PZASCE9772 / 220875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.