MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PolyLabs U36-5 Helmet Padding PU Foam
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: This medium density polyurethane foam is employed in helmet padding applications. This style also serves as beneficial in other padding applications not requiring a high tear resistance. U36-5 can be co-molded on fabric. It can also be in-mold coated. Either of these options will provide a more durable surface for the foam system.

Information provided by PolyLabs.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.300 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 14 - 16
@Time 10.0 sec
Tensile Strength 69.0 psi
Elongation at Break 183 %
Tear Strength 4.10 pliDie C
Compression Set 1.0 %
@Temperature 25.0 °C
% of original deflection after 50% set
 2.0 %
@Temperature 25.0 °C
% of original thickness after 50% set
 7.0 %
@Temperature 70.0 °C
% of original deflection after 50% set
 14 %
@Temperature 70.0 °C
% of original thickness after 50% set
 
Descriptive Properties
Trouser Tear (p/l)4.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYLA983 / 265879

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.