MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Titanium Ti-4Al-3Mo-1V
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Alpha-beta alloy. Available as plate and sheet. Tensile properties are for STA condition.

Key Words: Ti-431
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1275 MPa
Tensile Strength, Yield 1100 MPa0.2% offset
Elongation at Break 3.0 - 5.0 %
Creep Strength 241 MPa
@Temperature 425 °C,
Time >=720000 sec
strain 0.15%
 448 MPa
@Temperature 425 °C,
Time >=720000 sec
strain 0.5%
 551 MPa
@Temperature 315 °C,
Time >=720000 sec
strain 0.09%
 689 MPa
@Temperature 315 °C,
Time >=720000 sec
strain 0.18%
Tensile Modulus 117 GPa
Ultimate Bearing Strength 2300 MPae/D = 2.0
Bearing Yield Strength 1900 MPae/D = 2.0
Shear Strength 950 MPa
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 4.0 %
Molybdenum, Mo 3.0 %
Titanium, Ti 92 %
Vanadium, V 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Sn-2Zr-2Mo-2Cr-.25Si Alpha-Beta Processed + Aged
Titanium IMI 367 (Ti-6Al-7Nb)
Titanium Ti-6Al-4V (Grade 5), STA
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Alpha-Beta Processed
Titanium Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti-17) Beta Processed

MTP431 / 142962

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.