MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Annulus Fibrosus
Categories: Wood and Natural Products

Key Words: cartilage, tendon, ligament, bone
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 110 MPa16000 psiparallel to fibers, specimen 2x2.5mm cross section, 6.5mm length
Tensile Strength, Yield 0.187 MPa27.1 psiperpendicular to lamellae, specimen 7.5x2.5mm cross section, 4.5mm length
Tensile Modulus 3.41 GPa495 ksiparallel to fibers
 3.54 GPa513 ksiHorizontal, specimen 2x1.5mm cross section, 15-25mm length

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Femur
Human Compact Bone, Haversian System
Mercury (II) Oxide, HgO (Montroydite)
Aremco Corr-Paintâ„¢ CP2050-XX High Temperature Protective Coating Epoxy-Phenolic, Glass Fiber Filled
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite

PTSXBI34 / 71520

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.