System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Lubrizol Pellethane® 2363-80AE Thermoplastic Polyurethane Elastomer
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Ether Grade
Material Notes:
Features: USP Class VI
Available in Americas, Europe, Middle East, Africa, India and Asia
Data provided by Lubrizol
Lubrizol acquired the Pellethane product line from Dow in 2009.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.12
g/cc
ASTM D792
Linear Mold Shrinkage
0.0050
-
0.0080
cm/cm
@Thickness 1.59 mm
plaque
Linear Mold Shrinkage, Transverse
-0.00100
-
0.0040
cm/cm
@Thickness 1.59 mm
plaque
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 224 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore A
81 - 89
ASTM D2240
Tensile Strength, Ultimate
28.9
MPa
ASTM D412
Elongation at Break
550 %
ASTM D412
50% Modulus
0.00480
GPa
@Strain 50 %
ASTM D412
100% Modulus
0.00610
GPa
@Strain 100 %
ASTM D412
300% Modulus
0.0103
GPa
@Strain 300 %
ASTM D412
Tear Strength
73.6
kN/m
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles
30
H22 Wheel, 1000g; ASTM D1044
Compression Set
30 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395 Method B
80 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395 Method B
Tensile Set
70 %
Elongation set after break; ASTM D412
Thermal Properties
Original Value
Comments
CTE, linear
165
µm/m-°C
@Temperature 20.0 °C
ASTM D696
Vicat Softening Point
81.7
°C
ASTM D1525
Glass Transition Temp, Tg
-47.0
°C
Processing Properties
Original Value
Comments
Melt Temperature
190
-
205
°C
Molding
190
-
205
°C
Extrusion
Mold Temperature
15.0
-
60.0
°C
Drying Temperature
80.0
-
95.0
°C
Compliance Properties
Original Value
Comments
USP Class VI
Yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Pellethane® 2363-80AE TPU
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-90AE Thermoplastic Polyurethane Elastomer
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
PDW288b / 138249
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.