MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Mocom (ALBIS) Altech® A 1000/110 IM PA6, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Conditioned; Polyamide 6; high impact modified, dry impact modified, easy release (demolding), high flow. Applications: housings, various

Information provided by ALBIS.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
@Time 86400 sec
0.012 - 0.014 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm
@Time 86400 sec
0.010 - 0.012 in/in
@Time 24.0 hour
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 MPa5080 psiISO 527-1/-2
Elongation at Yield 25 %25 %ISO 527-1/-2
Tensile Modulus 0.810 GPa117 ksiISO 527-1/-2
Flexural Strength 20.0 MPa2900 psiISO 178
Flexural Modulus 0.780 GPa113 ksiISO 178
Charpy Impact Unnotched 100 J/cm²476 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 10.0 J/cm²47.6 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 11357
 
Processing PropertiesMetricEnglishComments
Melt Temperature 250 - 270 °C482 - 518 °Finjection molding
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Moisture Content <= 0.0015 %<= 0.0015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® B3K PA6 (Conditioned)
BASF Ultramid® B3K PA6 (Dry)
Cast Nylons Nycast® 6MPB Plasticized Nylon 6
Overview of materials for Nylon 6, Unreinforced
BASF Ultramid® 1310-11 NF2001 PA66 (Conditioned)

PALBIS9911 / 221007

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.