MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Samyang TRIREX® 3026PJ(B1) PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Product Description: TRIREX is the registered trademark of polycarbonate resin manufactured by Samyang Corporation. TRIREX polycarbonate resins offer superior mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries. TRIREX 3026PJ(B1) is a polycarbonate resin grade which has high low temperature impact strength in combination with superior mechanical and physical property.
Characteristics: Superior low temperature impact resistance; Good flow-ability; Workable under a wide range of temperatures (-100-135°C); High electrical performance; Good dimensional stability; Low moisture absorbency; Good weather resistance
Applications: TRIREX 3026PJ(B1) resin grade is used for extrusion blow molding components. High viscosity. Transparent colors only.

Availability: Asia Pacific; Europe; North America

Features: Good Dimensional Stability; Good Electrical Properties; Good Flow; Good Weather Resistance; Low Moisture Absorption; Low Temperature Impact Resistance; High Viscosity

Uses: Appliances; Automotive Applications; Electrical/Electronic Applications; Optical Applications

Appearance: Clear/Transparent

Form: Pellets

Processing Method: Extrusion Blow Molding

Information provided by Samyang Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Water Absorption <= 0.15 %
@Time 86400 sec
ASTM D570
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.00 mm
ASTM D955
Melt Flow 2.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10300 psiASTM D638
Elongation at Break 150 %ASTM D638
Flexural Yield Strength 13200 psiASTM D790
Flexural Modulus 331000 psiASTM D790
Izod Impact, Notched 17.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+16 ohm-cmASTM D257
Dielectric Strength 760 V/milASTM D149
Arc Resistance >= 120 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 28.0 - 39.0 µin/in-°FASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 273 °FUnannealed; ASTM D648
Flammability, UL94 V-2
@Thickness 1.52 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 473 - 518 °F
Middle Barrel Temperature 500 - 545 °F
Front Barrel Temperature 527 - 572 °F
Nozzle Temperature 527 - 590 °F
Melt Temperature 527 - 590 °F
Mold Temperature 149 - 221 °F
Drying Temperature 248 °F
Dry Time 3.00 - 5.00 hour
Back Pressure 36.3 - 102 psi
Vent Depth 0.000790 - 0.00310 in
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSAMY11457 / 312150

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.