MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese AT 416 Low Density Polyethylene (LDPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: AT 416 resin is well suited for extrusion coating and lamination applications such as envelope stock and thin paper coatings. This resin has excellent adhesion and high line speed capability. This polymer may be processed on conventional extrusion equipment. A melt temperature in the 270-310°C range is recommended for this resin.

Applications: Extrusion Coating & Laminating

Information provided by Celanese Corporation.

Key Words: extrusion coating and lamination applications such as envelope stock and thin paper coatings
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccAT Plastics PTM-03
Thickness >= 5.00 micronsCoating Thickness
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Coating Weight 3.00 lb/ream
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9.00 MPaType IV (50 mm/min); ASTM D638
Elongation at Break 500 %Type IV (50 mm/min); ASTM D638
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °CASTM D1525
 
Descriptive Properties
Line Speed ft/min< 1500

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Low Density Polyethylene (LDPE), Molded
Mitsubishi Chemical Advanced Materials Proteus™ LDPE Low Density Polyethylene
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
Celanese AT 253 Low Density Polyethylene (LDPE)

PATEVB29 / 25985

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.