MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and good abuse resistance. It can be used as a sealant layer in multilayer film structures for dry and liquid packaging.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccASTM D792
Thickness 0.800 mil
Melt Flow 3.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1440 psiASTM D882
Film Tensile Strength at Yield, TD 790 psiASTM D882
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 570 %ASTM D882
Secant Modulus, MD 0.108 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.115 GPa2% Secant; ASTM D882
Impact 10.7[lbf]; Puncture Resistance Force; Dow Method
 380[ft-lbf/in3]; Puncture Resistance; Dow Method
Puncture Energy 37.9 in-lbDow Method
Elmendorf Tear Strength MD 120 gModified rectangular test specimen; ASTM D1922
Elmendorf Tear Strength TD 410 gModified rectangular test specimen; ASTM D1922
Elmendorf Tear Strength, MD 150 g/milASTM D1922
Elmendorf Tear Strength, TD 512.5 g/milASTM D1922
Dart Drop Test >= 830 gMethod B; ASTM D1709
Film Tensile Strength at Break, MD 6470 psiASTM D882
Film Tensile Strength at Break, TD 4320 psiASTM D882
Heat Seal Strength Initiation Temperature 94.0 °C1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 98.0 °CDow Method (DSC)
Vicat Softening Point 85.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 0.70 %ASTM D1003
Gloss 144 %20°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow AFFINITY™ EG 8100G Ethylene-octene copolymer
Dow AFFINITY™ PL 1840G Polyolefin Plastomer (POP)
Dow AFFINITY™ EG 8100 Polyolefin Elastomer
Dow AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)

PDOW1174 / 30392

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.