MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Eastman Triacetin Plasticizer
Categories: Other Engineering Material

Material Notes: Product Description: Eastman™ Triacetin is used as a plasticizer for cellulosic resins and is compatible in all proportions with cellulose acetate, nitrocellulose, and ethyl cellulose. Eastman™ Triacetin is useful for imparting plasticity and flow to laminating resins, particularly at low temperatures, and is also used as a plasticizer for vinylidene polymers and copolymers. It serves as an ingredient in inks for printing on plastics, and as a plasticizer in nail polish. For food additive applications, Eastman supplies Eastman™ Triacetin, Kosher, Food Grade, and Eastman™ Triacetin, Food Grade, which are made under appropriate current good manufacturing practices (cGMP) for these applications.

Application/Uses:

  • Coatings
  • Decals/Graphics/Graphic Arts
  • EVA water based adhesives
  • Pressure sensitive adhesives
  • PVAc water based adhesives

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/cc
Viscosity 17.4 cP
Vapor Pressure <= 0.00000329 atm
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 0.0020
 
Thermal PropertiesOriginal ValueComments
Melting Point 37.8 °CFreezing Point
Boiling Point 258 °C
Flash Point 151 °CSetaflash Closed Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.43
 
Descriptive Properties
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5261 / 222455

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.