MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CHT ALPATEC 114 1 part adhesive and sealant, RVT silicone
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Acetoxy cure products which are solvent free. During cure, it liberates a very small amount of acetic acid, giving rise to the familiar ‘vinegar’ odour, which quickly dissipates after cure. It exhibits good primer-less adhesion to many substrates including but not limited to; aluminium, nonferrous metals, steel, glass, enamelled surfaces, fabrics ceramics, thermosetting, thermoplastics and wood and cures rapidly at room temperature when in contact with atmospheric moisture. This product is not to be recommended for use with galvanized metals, ferrous metals, copper and its associated alloys or in electronic assemblies.

Key Features

  • Permanently temperature stable up to 250 °C/482°F, shortly up to 350 °C/662°F
  • Very good stability to motor oils and coolants
  • For producing heat insulation elements
  • For bonding oven windows
Key Applications:
  • FIPG (Formed In Place Gasket) as wet and dry sealing in motor production(oil pans, valve bonnets etc.) li>For sealing building components and devices which are exposed to high temperatures
Application: Where stability with motor oils and coolants is needed, heat insulation elements, bonding oven windows, building components and devices which are subject to high temperatures, FIPG, oil pans, valve bonnets wet and dry sealing

Cured Product: Standard climate DIN 50 014 - 23/50-2. Vulcanizate tested after 14 days

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³uncured; DIN 53 479, 23
Storage Temperature 5.00 - 30.0 °C41.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050DIN 53 505
Tensile Strength 2.60 MPa377 psiDIN 53 504, S 3 A
Elongation at Break 300 %300 %DIN 53 504, S 3 A
Modulus of Elasticity 0.000250 GPa
@Strain 100 %
0.0363 ksi
@Strain 100 %
DIN 53 504, S 3 A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorAnthracite
Cure typeAcetate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL000 / 314483

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.