MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Magnesium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 - 2.40 g/cc0.0480 - 0.0867 lb/in³Average value: 1.81 g/cc Grade Count:160
Porosity 0.000 - 1.10 %0.000 - 1.10 %Average value: 0.550 % Grade Count:3
Particle Size 0.000 - 2800 µm0.000 - 2800 µmAverage value: 974 µm Grade Count:10
Vapor Pressure 1.51987e-020 bar1.00e-17 torrAverage value: 1.51987e-020 bar Grade Count:4
 
Chemical PropertiesMetricEnglishComments
Thermal Neutron Cross Section 0.0600 barns/atom0.0600 barns/atomAverage value: 0.0600 barns/atom Grade Count:4
Electrode Potential -2.37 V-2.37 VAverage value: -2.37 V Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 30.0 - 11830.0 - 118Average value: 63.7 Grade Count:96
Hardness, Knoop 67.0 - 11367.0 - 113Average value: 87.3 Grade Count:53
Hardness, Rockwell A 35.0 - 37.535.0 - 37.5Average value: 36.1 Grade Count:5
Hardness, Rockwell B 49.0 - 55.049.0 - 55.0Average value: 52.0 Grade Count:6
Hardness, Rockwell E 59.0 - 88.059.0 - 88.0Average value: 72.5 Grade Count:32
Hardness, Vickers 55.0 - 10555.0 - 105Average value: 79.0 Grade Count:56
Tensile Strength, Ultimate 90.0 - 515 MPa13100 - 74700 psiAverage value: 251 MPa Grade Count:156
Tensile Strength, Yield 21.0 - 460 MPa3050 - 66700 psiAverage value: 165 MPa Grade Count:154
Elongation at Break 1.00 - 30.5 %1.00 - 30.5 %Average value: 8.47 % Grade Count:154
Modulus of Elasticity 38.0 - 120 GPa5510 - 17400 ksiAverage value: 45.2 GPa Grade Count:138
Compressive Yield Strength 21.0 - 465 MPa3050 - 67400 psiAverage value: 179 MPa Grade Count:110
Notched Tensile Strength 230 - 260 MPa33400 - 37700 psiAverage value: 250 MPa Grade Count:3
Ultimate Bearing Strength 250 - 585 MPa36300 - 84800 psiAverage value: 443 MPa Grade Count:47
Bearing Yield Strength 125 - 515 MPa18100 - 74700 psiAverage value: 314 MPa Grade Count:47
Poissons Ratio 0.250 - 0.3500.250 - 0.350Average value: 0.338 Grade Count:135
Fatigue Strength 15.0 - 235 MPa2180 - 34100 psiAverage value: 95.1 MPa Grade Count:55
Fracture Toughness 13.2 - 34.0 MPa-m½12.0 - 30.9 ksi-in½Average value: 18.8 MPa-m½ Grade Count:12
Machinability 100 %100 %Average value: 100 % Grade Count:57
Shear Modulus 16.3 - 48.0 GPa2360 - 6960 ksiAverage value: 17.2 GPa Grade Count:123
Shear Strength 55.0 - 200 MPa7980 - 29000 psiAverage value: 144 MPa Grade Count:72
Charpy Impact 0.680 - 6.10 J0.502 - 4.50 ft-lbAverage value: 2.48 J Grade Count:36
Charpy Impact, Unnotched 7.46 - 16.6 J5.50 - 12.3 ft-lbAverage value: 10.9 J Grade Count:5
Coefficient of Friction 0.3600.360Average value: 0.360 Grade Count:4
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000460 - 0.000110 ohm-cm0.00000460 - 0.000110 ohm-cmAverage value: 0.0000106 ohm-cm Grade Count:130
Magnetic Permeability 1.001.00Average value: 1.00 Grade Count:4
Magnetic Susceptibility 5.50e-75.50e-7Average value: 5.50e-7 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 13.8 - 28.0 µm/m-°C7.67 - 15.6 µin/in-°FAverage value: 26.5 µm/m-°C Grade Count:146
Specific Heat Capacity 0.800 - 1.45 J/g-°C0.191 - 0.346 BTU/lb-°FAverage value: 1.02 J/g-°C Grade Count:135
Thermal Conductivity 44.3 - 159 W/m-K307 - 1100 BTU-in/hr-ft²-°FAverage value: 91.1 W/m-K Grade Count:127
Melting Point 330 - 650 °C626 - 1200 °FAverage value: 540 °C Grade Count:126
Solidus 330 - 650 °C626 - 1200 °FAverage value: 533 °C Grade Count:117
Liquidus 585 - 650 °C1090 - 1200 °FAverage value: 626 °C Grade Count:118
Boiling Point 1090 °C1990 °FAverage value: 1090 °C Grade Count:5
Maximum Service Temperature, Air 150 - 300 °C302 - 572 °FAverage value: 219 °C Grade Count:7
Deflection Temperature at 1.8 MPa (264 psi) 371 °C700 °FAverage value: 371 °C Grade Count:3
Ignition Temperature 482 °C900 °FAverage value: 482 °C Grade Count:3
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.07000.0700Average value: 0.0700 Grade Count:4
Reflection Coefficient, Visible (0-1) 0.720 - 0.9300.720 - 0.930Average value: 0.804 Grade Count:4
 
Processing PropertiesMetricEnglishComments
Processing Temperature 230 - 705 °C446 - 1300 °FAverage value: 435 °C Grade Count:27
Annealing Temperature 345 - 455 °C653 - 851 °FAverage value: 377 °C Grade Count:20
Casting Temperature 640 - 850 °C1180 - 1560 °FAverage value: 753 °C Grade Count:52
Recrystallization Temperature 345 - 455 °C653 - 851 °FAverage value: 376 °C Grade Count:7
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.500 - 51.6 %0.500 - 51.6 %Average value: 7.05 % Grade Count:91
Beryllium, Be 0.000800 %0.000800 %Average value: 0.000800 % Grade Count:4
Calcium, Ca 0.0400 - 0.300 %0.0400 - 0.300 %Average value: 0.142 % Grade Count:14
Copper, Cu 0.0100 - 3.00 %0.0100 - 3.00 %Average value: 0.209 % Grade Count:89
Gadolinium, Gd 1.00 - 25.0 %1.00 - 25.0 %Average value: 8.40 % Grade Count:3
Iron, Fe 0.00350 - 0.150 %0.00350 - 0.150 %Average value: 0.0145 % Grade Count:30
Lithium, Li 0.200 - 15.0 %0.200 - 15.0 %Average value: 7.10 % Grade Count:4
Magnesium, Mg 48.0 - 100 %48.0 - 100 %Average value: 92.9 % Grade Count:198
Manganese, Mn 0.0800 - 1.20 %0.0800 - 1.20 %Average value: 0.354 % Grade Count:102
Neodymium, Nd 0.600 - 28.0 %0.600 - 28.0 %Average value: 4.98 % Grade Count:16
Nickel, Ni 0.00100 - 0.0300 %0.00100 - 0.0300 %Average value: 0.00941 % Grade Count:87
Rare Earths 0.100 - 22.0 %0.100 - 22.0 %Average value: 3.88 % Grade Count:24
Silicon, Si 0.0100 - 1.50 %0.0100 - 1.50 %Average value: 0.259 % Grade Count:74
Silver, Ag 1.30 - 3.00 %1.30 - 3.00 %Average value: 2.12 % Grade Count:11
Thorium, Th 0.600 - 4.00 %0.600 - 4.00 %Average value: 2.58 % Grade Count:14
Yttrium, Y 3.70 - 28.0 %3.70 - 28.0 %Average value: 7.41 % Grade Count:14
Zinc, Zn 0.120 - 7.00 %0.120 - 7.00 %Average value: 2.01 % Grade Count:125
Zirconium, Zr 0.200 - 38.0 %0.200 - 38.0 %Average value: 1.25 % Grade Count:56

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Aluminum Alloy
Magnesium, Mg; Hard-Rolled Sheet
Magnesium, Mg; Annealed Sheet
Overview of materials for Nickel Alloy
Overview of materials for Copper Alloy

M01059 / 81672

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.