High Impact, High Surface Quality ABS Sheet (Low Gloss) ALLEN® AXL/LXS is general purpose ABS that has high impact strength and superior surface quality. ALLEN® AXL/LXS is Underwriters Laboratories, Inc® recognized for UL Std 94 HB (UL94) and Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302) Suggested Applications: - Decorative Lamination
- Critical Surface Quality for Painting
- Vehicle Interior
Features: - Good forming properties
- Edge trim easily used into future orders
- Excellent surface quality
- Low gloss finish
Information provided by Sekisui Polymer Innovations |