MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ametek AM 388™ Alloy (UNS C72650) TD04 Hard
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Information supplied by Ametek Specialty Metal Products Division.

Copper base Spinodal alloy with high conductivity and high strength. Outstanding performance for contacts in connectors, sockets and switches.

Benefits include combination of high strength and formability, high conductivity, available in mill hardened or age hardenable tempers, no distortion during aging, no fixturing required, excellent solderability and resistance to stress relaxation during high temperature (over 400°F, 200°C) soldering, fine grain size, excellent corrosion resistance bare and easy to plate when required, low initial cost, and additional savings during processing.

Aging Temperature/Time 700°F-725°F (370°C-385°C)/1.5-3 hrs.

Key Words: Copper Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.87 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 200 - 240200 - 240
Tensile Strength, Ultimate 586 - 655 MPa85000 - 95000 psi
Tensile Strength, Yield 551 - 620 MPa
@Strain 0.2 %
79900 - 89900 psi
@Strain 0.2 %
Elongation at Break 2.0 - 5.0 %2.0 - 5.0 %typical
Modulus of Elasticity 124 GPa18000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000115 - 0.0000123 ohm-cm0.0000115 - 0.0000123 ohm-cmConductivity 14 - 15% IACS
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 87 %87 %as balance
Nickel, Ni 7.0 - 8.0 %7.0 - 8.0 %
Other <= 0.50 %<= 0.50 %
Tin, Sn 4.5 - 5.5 %4.5 - 5.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Crucible Steel AISI 52100 Alloy Steel

NMA259 / 18178

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.