MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Vibrantz Technologies EG 2739 Thick Film Glass
Categories: Ceramic; Glass

Material Notes: Glass Type: Pb-Zn-B
Typical Powder Form: MVG
Typical Application: Resistor Overglaze

Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conductors, end terminations, over glazes, and dielectrics.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 5.15 g/cc0.186 lb/in³
Particle Size 5.0 µm5.0 µm50% of particles
 <= 25 µm<= 25 µm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.25 µm/m-°C4.58 µin/in-°Fat Set Pt.
 7.00 µm/m-°C
@Temperature 260 °C
3.89 µin/in-°F
@Temperature 500 °F
Softening Point 478 °C892 °F
Annealing Point 420 °C788 °F
Transformation Temperature 400 °C752 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 500 °C932 °FTypical Firing Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CFERR63 / 877

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.