MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Prodways PLASTCure Clear 200 Liquid Resin for 3D Printing
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic

Material Notes: Adapted to the manufacturing of parts requiring high transparency, PLASTCure Clear materials meet requirements for a wide range of applications in medical 3D printing such as surgical modeling.

Designed for UV photo-polymerization in DLP printers.

Information provided by Prodways

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccLiquid
Water Absorption 0.50 - 0.70 %ASTM D570
Viscosity 500 - 700 cP
@Temperature 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 66.0 - 71.0 MPaASTM D638
Elongation at Break 3.0 - 4.0 %ASTM D638
Tensile Modulus 2500 - 2900 MPaASTM D638
Flexural Strength 110 - 120 MPaASTM D790
Flexural Modulus 2500 - 2700 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 - 69.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Clear" but manufacturer doesn't quantify.
 
Descriptive Properties
AppearanceClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Prodways PLASTCure Clear 100 3D Printing Polymer
Prodways PLASTCure ABS 2800 Liquid Resin for 3D Printing
EOS PH1 Precipitation Hardening Stainless Steel Sintered on EOSINT M 270
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr

PPRODW970 / 220988

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.